How to Choose the Right Nylon: A Systematic Material Selection Guide

Selecting the correct nylon grade is one of the most consequential decisions in engineering plastics procurement. A wrong choice — choosing PA66 where PA6 suffices, or specifying unfilled nylon for a structural application — can result in field failures, production delays, and costly material substitutions mid-project.
This guide provides a structured decision framework based on actual engineering criteria: mechanical requirements, thermal environment, moisture exposure, chemical contact, regulatory compliance, and cost. Every selection factor is tied to real-world data so you can make evidence-based decisions, not rely on generic rule-of-thumb guidance.

The Five Critical Selection Criteria
Before examining specific grades, establish the priority order of these five criteria for your application. Most applications fail because two or more criteria conflict — understanding which takes precedence avoids costly design changes later.
| Criterion | Pourquoi est-ce important ? | Primary Impact | Secondary Impact |
|---|---|---|---|
| Mechanical Strength | Load-bearing capacity required | Structural parts, brackets | Gear teeth, bearing surfaces |
| Résistance thermique | Maximum service temperature | Engine components, high-heat zones | Processing window |
| Moisture Sensitivity | Operating humidity environment | Dimensional stability | Electrical properties |
| Exposition à des produits chimiques | Fluids in contact with part | Fuel, oil, acid, alkali | Cleaning agents, solvents |
| Regulatory Compliance | Market and industry standards | Food, medical, potable water | Automotive, aerospace |
PA6 vs. PA66: The Fundamental Choice
PA6 and PA66 together account for over 90% of global nylon consumption. Understanding their differences is the foundation of all material selection decisions.
| Propriété | PA6 | PA66 | Winner |
|---|---|---|---|
| Point de fusion | 220-225°C | 260-265°C | PA66 |
| Crystallinity | Lower (~40%) | Higher (~50%) | PA66 for dimensional stability |
| Résistance à la traction | 70-85 MPa | 80-90 MPa | PA66 |
| Résistance aux chocs | Higher (tougher) | Lower (stiffer) | PA6 |
| Rétrécissement du moule | 1.0-1.5% | 1.3-1.8% | PA6 (lower warpage) |
| Water Absorption | 8.5-9.0% | 8.0-8.5% | Similar |
| Température de traitement | 230-260°C | 270-295°C | PA6 (lower energy) |
| Coût | Plus bas | Plus élevé | PA6 (20-30% cheaper) |
| Fatigue Resistance | Bon | Excellent | PA66 |
Reinforced Grades: When to Specify Glass or Carbon Fiber
Unreinforced nylon serves many applications well, but structural, high-temperature, and high-precision applications almost always require reinforcement. GF30 and GF33 (glass fiber) are the workhorses; CF30 (carbon fiber) is selected for ultra-lightweight or high-stiffness applications.
| Grade | Résistance à la traction | Module de flexion | HDT (1,82 MPa) | Avantage clé | Applications typiques |
|---|---|---|---|---|---|
| PA6 (non chargé) | 70-85 MPa | 2,800 MPa | 70°C | Tough, cost-effective | Gears, bushes, flexible parts |
| PA66 (non chargé) | 80-90 MPa | 3,000 MPa | 80°C | Stiff, fatigue-resistant | Structural parts, bearings |
| PA6-GF30 | 160-180 MPa | 8,500 MPa | 215°C | Heat resistant, stiff | Engine covers, brackets |
| PA66-GF33 | 190-210 MPa | 10,500 MPa | 250°C | Highest stiffness | Structural automotive |
| PA6-GF50 | 200-230 MPa | 15 000 MPa | 220°C | Metal replacement | Heavy-load brackets |
| PA66-CF30 | 240-280 MPa | 20,000 MPa | 260 °C | Lightweight, ESD-safe | Robotics, aerospace |
| PA12 (unfilled) | 45-55 MPa | 1,800 MPa | 85°C | Low moisture, flexible | Fluid systems, catheters |
Moisture and Environment: Matching to Operating Conditions
Moisture absorption is the most misjudged selection factor. Engineers often underestimate how dramatically water plasticizes nylon, reducing modulus by 40% and increasing dimensions significantly.
| Operating Environment | Niveau recommandé | Why | Alternative |
|---|---|---|---|
| Dry interior (<50% RH) | PA66 | Dimensional accuracy, stiffness | PA6 |
| Humid interior (50-80% RH) | PA66-GF30 | Moisture-stable when reinforced | PA6-GF30 |
| Outdoor exposed | PA66-GF30 + UV | UV stabilization essential | PA12 |
| Under-hood automotive | PA66-HT or PA66-GF30 | Heat-stabilized for >150°C | PA6-GF30 |
| Potable water contact | PA66-GF30 or PA12 | NSF/ANSI 61 compliant grades | PA66 approved |
| Chemical plant | PA66 or PVDF | Acid/alkali resistant grades | PP or HDPE |
| Low temperature (-30°C) | PA66 | Retains toughness at low temps | PA66-GF30 |
| High temperature (>200°C) | PA66-GF30 or PPA | Beyond PA66 capacity | PEEK or PPS |
Application-Specific Selection Matrix
Rather than selecting by property alone, match the material to the application category for the fastest path to the right grade.
| Application Category | L'industrie | Recommended Nylon | Certification Needed |
|---|---|---|---|
| Air intake manifolds | Automobile | PA66-GF30 + heat stabilizer | OEM approval, under-hood thermal |
| Fuel rails and lines | Automobile | PA66-GF30 or PA12 | EN 594, SAE emissions |
| Electrical connectors | E&E, Automotive | PA66 V-0, PA6 V-2 | UL 94, IEC 60335 |
| Beverage tubing and fittings | Food & Beverage | PA12, PA66 food-grade | FDA 21 CFR 177.1500, EU 10/2011 |
| Medical device housings | Médical | PA66 medical-grade | ISO 10993, FDA 510(k) |
| Industrial gears and bearings | Machinery | PA66-GF30 or PA66-CF30 | None mandatory |
| Sports equipment | Consumer | PA6, PA66 | REACH, CPSIA for toys |
| Drone structural frames | Robotics/Aero | PA66-CF30 | UL 94 V-0 if electrical |
FAQ

When does Nylon (PA) Material Selection Guide for Injection Molding make sense?
Nylon (PA) Material Selection Guide for Injection Molding makes sense when the part volume, material choice, geometry, and repeatability needs justify mold design and tooling investment.
What design factors matter most for Nylon (PA) Material Selection Guide for Injection Molding?
L'épaisseur des parois, les nervures, les bossages, l'angle de dépouille, l'emplacement de l'entrée de matière, le retrait, la ligne de joint et l'éjection sont autant de facteurs qui influent sur la qualité des pièces moulées.
Quelles informations faut-il fournir avant la fabrication d'un moule ?
Le fournisseur doit confirmer le modèle 3D, le matériau, le volume annuel prévu, les exigences en matière d'aspect, les tolérances requises, ainsi que toute exigence relative à l'assemblage ou aux essais fonctionnels.
What is the biggest risk in Nylon (PA) Material Selection Guide for Injection Molding?