PA6 GF GB30 usually refers to a PA6 molding compound with both chopped glass fiber and glass beads. Buyers compare it with fiber-only PA6 when a molded cover, enclosure or locating feature needs stiffness together with controlled warpage. Confirm the producer’s designation, the glass split and the actual part requirements before ordering.

Qu'est-ce que le PA6 GF GB30 ?
GF denotes glass fiber and GB denotes glass beads. For example, BASF identifies Ultramid B3GK24 Uncolored as PA6-(GF+GB)30, a combined glass-fiber and glass-bead reinforced molding grade. In that designation, 30 identifies the combined filler loading by mass. It does not specify bead diameter or the split between fibers and beads. Confirm how the producer of the quoted grade uses its code.
À propos de notre offre de plastiques techniques
For a resin enquiry, provide the required formulation, color, quantity and application. For a molded part, include the drawing and the defect or fit problem you are trying to solve. Request documents for the actual supplier, grade and production location where applicable.
En quoi les billes de verre et les fibres de verre diffèrent-elles en matière de renforcement ?

| Filler | Typical role | What to request |
|---|---|---|
| Chopped glass fiber | Stiffens the compound, with reinforcement influenced by flow direction | Mechanical data in relevant directions and evidence at critical weld lines |
| Glass beads | A spherical filler that can alter the shrinkage balance of a formulation | Flow and transverse shrinkage values and molded-part flatness |
| Glass fiber plus glass beads | Lets the producer tune a balance of stiffness and dimensional behavior | Exact grade and filler breakdown if available, plus actual-part molding results |
What Can a Hybrid Grade Improve?

A hybrid grade is worth testing when the fiber-only baseline meets load requirements but leaves a warped sealing face, uneven seam or cosmetic problem. Spherical beads have no long axis, but fibers in the same compound still orient with flow. Gate location, packing, cooling and wall layout also affect final shape.
Compare samples in the same tool under agreed molding and conditioning states. Record flatness, mating gap, visible surface, impact and load performance. Gloss, injection pressure and cycle time require their own checks.
Propriétés mécaniques, thermiques et dimensionnelles
| Propriété | Données à comparer |
|---|---|
| Stiffness, strength and impact | Current TDS for the quoted compound, with test method, conditioning and orientation |
| HDT and heat aging | Test load and specimen conditions for HDT, then retained properties under the actual duty cycle |
| Shrinkage, CLTE and fit | Flow and transverse values with measurement conditions, plus dimensions after relevant conditioning |
| Qualité de surface | A molded sample with the intended gate, color and surface texture |
Comparaison : PA6 GF30, PA6 GF GB30 et PA6 GB30
| Grade strategy | When to evaluate it | Decision evidence |
|---|---|---|
| PA6 GF30 | Load-bearing baseline with about 30% glass fiber when specified by the supplier | Confirm strength and stiffness in the load direction and check warp around interfaces |
| PA6 GB30 | Bead-filled candidate when appearance or fit dominates | Confirm bead loading, impact and the load capacity of the actual part |
| PA6-(GF+GB)30 | Hybrid candidate when the existing grade has a measurable flatness or assembly issue | Compare two grade samples against the same dimensional, cosmetic and mechanical criteria |
Applications typiques

Consider a hybrid compound for covers, locator features and multi-piece housings where distortion changes the assembled gap. Separate a cosmetic cover from a pressure-carrying, high-heat or electrically rated part. The latter needs its own fluid, heat-aging, pressure or electrical verification for the exact grade and geometry.
Consignes de transformation pour les composés chargés de GF et de GB

Set drying and residual moisture from the grade instructions. Use the recommended melt and mold windows, then qualify filling, packing and cooling on the actual mold. Check gates, vents, wear surfaces and ejector access with the toolmaker.
Before releasing the material, agree how to compare warp, weld-line performance, assembly fit and appearance. For a part or mold review, send the drawing, annual volume, current material, defect photos and the relevant load and conditioning requirements. Review injection molding options ou Request a grade comparison.
FAQ
Does GB30 mean a 30-micrometer glass bead?
No. Check the supplier’s notation. In a designation such as PA6-(GF+GB)30, the 30 identifies the combined filler loading. Bead size and the fiber-to-bead split require separate supplier data.
Will the hybrid grade remove warpage?
It may change the balance of shrinkage. Compare an actual molding in the same tool and verify flatness and fit in the specified conditioning state.
Can PA6-(GF+GB)30 replace PA6 GF30 directly?
Compare the exact grades for strength, impact, shrinkage, moisture response and processing. Confirm the tool and the assembly before approving the substitution.
What should the supplier quote include?
Ask for the grade designation, current TDS, sample quantity and intended molding conditions. Include the drawing, critical datums, annual volume and the failure or defect to resolve.
Lire la suite
- Polypropylène renforcé de fibres de verre : Un guide complet des matériaux PP GF pour l'automobile et l'industrie
- Fibre de verre : Guide complet des composites à base de polymères renforcés par des fibres
- Matériau PA6 : Guide complet sur les propriétés, la mise en œuvre et les applications du nylon 6
Pourquoi choisir le plastique nylon ?
Nylon Plastic supports PA6 reinforced-grade review when stiffness, dimensional control and procurement risk need to be balanced for production.