Nylon 6 vs Nylon 66 injection molding compares the two material families for molded parts by processing window, heat, stiffness, impact, moisture, shrinkage and cost.
Nylon 6 or Nylon 66: Start with the Service Condition
Moisture condition, reinforcement and the exact commercial grade can change this decision. Use the comparison below as a screening step, then validate the selected grade on the actual part.
When specifying nylon for injection molded parts, the choice between Nylon 6 (PA6) and Nylon 66 (PA66) is one of the most consequential decisions an engineer can make. While chemically similar, the difference of one carbon atom in the monomer structure creates a cascade of divergent properties that ripple through every stage of production and part performance.
This guide goes beyond standard datasheet comparisons. We examine how PA6’s broader processing window and superior impact performance stack up against PA66’s higher heat deflection temperature and stiffness, and what each trade-off costs you in practice.

Molecular Architecture: Why the Extra Carbon Matters
The performance divergence originates at the molecular level. Nylon 6 is polymerized from caprolactam, producing chains with amide groups spaced every six carbons. Nylon 66 is formed from hexamethylene diamine and adipic acid, creating chains where the amide density is identical but hydrogen bonding patterns differ.

This structural distinction gives PA66 a melting point of 255-265°C versus PA6’s 220°C. The tighter crystalline packing results in 15-25% higher tensile strength and flexural modulus at room temperature. However, PA6’s chain mobility provides 2-3× better notched Izod impact resistance, especially at low temperatures where PA66 can become brittle.
Processing: Moldability vs Mechanical Properties
The processing window is where PA6 often wins in production. With a melt temperature range of 230-270°C versus PA66’s 260-300°C, Nylon 6 reduces energy costs and extends barrel life. Its broader crystallization window means less sensitivity to mold temperature variations in multi-cavity tools.

| Propriété | PA6 (Nylon 6) | PA66 (nylon 66) | Pourquoi est-ce important ? |
|---|---|---|---|
| Point de fusion | 220°C | 255-265°C | PA6 requires lower barrel temps, reducing degradation risk |
| Résistance à la traction (à l'état sec) | 70 à 85 MPa | 80-95 MPa | PA66 ~12% stronger dry; gap narrows when conditioned |
| Module de flexion (à l'état sec) | 2.6-3.0 GPa | 2.8-3.3 GPa | PA66 stiffer; critical for structural brackets |
| Résistance au choc Izod avec entaille | 5-8 kJ/m² | 3-5 kJ/m² | PA6 clear winner for snap-fits and impact-prone parts |
| Rétrécissement du moule | 0.5-1.5% | 1.0-2.0% | PA6 holds tighter tolerances; less draft needed |
| Moisture (24h) | 2.5-3.0% | 2.0-2.5% | PA66 absorbs slightly less; more stable in humidity |
| HDT à 1,8 MPa | 65-80°C | 80-100 °C | PA66 handles 15-20°C higher heat; under-hood ready |
Moisture Conditioning: The Hidden Variable
When conditioned to equilibrium (50% RH, 23°C), PA6 tensile drops to 35-45 MPa with dramatically improved impact resistance (15-25 kJ/m² Izod). PA66 conditioned reaches 55-65 MPa with more modest impact gains. Dry-as-molded PA6 parts can be dangerously brittle until they absorb atmospheric moisture—typically 40-90 days post-molding depending on wall thickness.

For parts that must ship immediately, PA66 offers a wider safety margin in the dry state. For snap-fit designs where impact resistance is paramount, PA6’s conditioned toughness makes it the better choice once hydrated.
Design Rules: Nylon 6 and 66
- Épaisseur de la paroi : 0.8-3.0 mm for PA6; 1.0-3.5 mm for PA66. Below 0.8 mm flow length becomes the bottleneck. Uniform walls essential—thickness variations >25% cause differential shrinkage warpage.
- Angle de tir : 0.5-1° minimum. PA66 requires more draft due to higher shrinkage. Textured surfaces: add 1° per 0.025 mm of texture depth.
- Rayon de courbure : Minimum 0.5 mm internal radius; 1.0 mm for PA66 to reduce stress concentration at knit lines.
- Emplacement de la porte : Position gates at the thickest section. PA66’s faster crystallization demands shorter fill times (<2 seconds for parts under 100g).
- Pré-séchage : Both hygroscopic. Dry to <0.15% moisture (80°C, 4-6h). Insufficient drying causes splay marks and 15-30% strength loss.
- Hole spacing: Edge distance ≥1.5× hole diameter. Closer spacing risks cracking at mold parting line, especially with PA66’s higher shrinkage.
Applications industrielles : les atouts de chaque nuance
| L'industrie | Pièces courantes | Note souhaitée | Justification du choix |
|---|---|---|---|
| Automobile | Engine covers, intake manifolds, radiator end tanks | PA66 GF30 | HDT 240°C withstands under-hood; glass fiber adds stiffness |
| Produits de consommation | Power tool housings, appliance gears, cable ties | PA6 | Better surface finish, lower cost, superior drop impact |
| Electrical | Connectors, circuit breakers, terminal blocks | PA66 V-0 | Higher RTI rating meets UL requirements |
| Machines industrielles | Gears, bearings, wear pads, conveyor components | PA6 + MoS₂ | Moly-filled PA6 offers excellent wear at lower cost |
| Food & Medical | Food processing components, pharma trays | PA6 | Better FDA-compliant availability, lower extractables |
Cadre de décision en matière de coûts
PA6 baseline: $2.80-3.50/kg vs PA66 : $3.50-4.50/kg. The raw material premium for PA66 is roughly 20-30%.


- Low volume (<1,000 pcs): Material cost difference negligible vs mold amortization. Choose on performance.
- Mid volume (1,000-50,000 pcs): PA6 saves $0.15-0.40/kg. For a 200g part at 50K/year, that’s $1,500-4,000 annual savings.
- High volume (>50,000 pcs): PA6’s faster cycle time (5-15% shorter) compounds with material savings for 8-12% lower total cost.
Hidden risk: PA66 supply is more volatile—historically subject to adiponitrile shortages. PA6 caprolactam supply is more diversified.
Problèmes courants et solutions
| Défaut | Aspect | Cause première | Solution |
|---|---|---|---|
| Splay marks | Silver streaks radiating from gate | Moisture >0.15% in resin | Verify dryer dew point <-30°C; extend drying to 6h at 80°C |
| Déformation | Part distortion, out-of-flat >0.5mm | Differential shrinkage; PA66 susceptible | Uniform wall thickness; add ribbing; increase mold temp 10-15°C |
| Brittle fracture | Parts crack on ejection or assembly | Dry-as-molded PA6; no conditioning | Condition in 80°C water bath 30 min or allow 40-90 day ambient aging |
| Faiblesse de la ligne de tricotage | Visible line, 30-50% strength loss | PA66 fast crystallization freezes melt fronts | Increase mold temp to 80-100°C; relocate gates from stress areas |
Pourquoi choisir le plastique nylon pour votre projet ?
Fabrication de précision
Plus de 30 cellules d'usinage CNC et de moulage par injection réunies sous un même toit
ISO 9001:2015
Système de qualité certifié, rapports d'inspection complets
Délai de livraison : 15 à 25 jours
Délais d'exécution rapides avec des options d'expédition accélérée disponibles
Livraison internationale
Fret aérien et maritime vers l'Amérique du Nord, l'Europe et l'Asie
Download Our Nylon Selection Guide
Guide de référence gratuit au format PDF comprenant des tableaux de sélection des matériaux, des règles de conception et des listes de contrôle pour l'évaluation des fournisseurs.
Questions fréquemment posées
Which is stronger, Nylon 6 or Nylon 66?
Nylon 66 is approximately 12-15% stronger in tensile strength and flexural modulus when dry (80-95 MPa vs 70-85 MPa). However, when conditioned to ambient humidity, the gap narrows significantly. For impact strength, Nylon 6 is 2-3× better, especially in cold environments where PA66 can become brittle.
Why does Nylon 6 absorb more water than Nylon 66?
The difference is about 0.5% at equilibrium—Nylon 6 absorbs ~2.5-3.0% while Nylon 66 absorbs ~2.0-2.5%. This stems from Nylon 6’s slightly more open crystalline structure, which creates more hydrogen bonding sites for water molecules. The practical effect: PA6 dimensions change more in humid environments, requiring wider tolerance allowances.
Can I use Nylon 6 instead of Nylon 66 to reduce cost?
Yes, in many applications the cost savings outweigh the performance gap. Evaluate your part’s maximum service temperature first: if it’s below 80°C continuous, Nylon 6 is almost always a viable substitute. For under-hood automotive (100-140°C) or structural components requiring maximum stiffness, PA66 remains the safer choice.
What is the recommended mold temperature for Nylon 6 vs 66?
Nylon 6 processes best at mold temperatures of 60-90°C, while Nylon 66 requires 80-120°C to achieve proper crystallinity. The higher mold temperature for PA66 means longer cycle times (5-15% more) and higher energy costs, but results in a part with better dimensional stability and mechanical properties.
Move from Material Choice to a Molded-Part Review
Share the drawing, service temperature, humidity, load, tolerance, reinforcement, quantity and document requirements. We can review the PA6 material route, PA66 material route et nylon injection molding process avant l'établissement du devis.
Lire la suite
- Nylon vs Polypropylene for Industrial Applications
- Glass-Filled Nylon: Complete Properties Guide
- Nylon Moisture Absorption: Effects on Properties
- CNC Machining vs Injection Molding Decision Guide
- Guide de sélection des matériaux en nylon (PA) pour le moulage par injection
- Guide de sélection des matériaux en nylon (PA) pour le moulage par injection
- Usinage CNC ou moulage par injection : comparaison complète des procédés de fabrication