Le guide complet des types de nylon : PA6, PA66, PA11, PA12 et bien d'autres encore

PA6, PA66, PA11, and PA12 nylon pellets and molded parts arranged for grade selection
Le choix d'une qualité de nylon adaptée est essentiel à la réussite d'un projet d'ingénierie

Nylon grades are selected in two steps: first choose the PA matrix, such as PA6, PA66, PA11, or PA12; then choose whether it remains unfilled or receives glass fiber, carbon fiber, impact, flame-retardant, wear, or other modification.

For the main commercial routes, unfilled PA is the baseline, GF20 adds moderate structural reinforcement, and CF30 targets higher specific stiffness or special electrical and dimensional requirements. The highest fiber percentage is not automatically the best grade.

Nylon Grade Selection at a Glance

First Decision Common Starting Point Motif
General molded part Unfilled PA6 or PA66 Toughness, wear, and processing balance
Moderate deflection control PA-GF20 More stiffness with a broader balance than higher loading
Structural molded part PA-GF30 Common stiffness and dimensional-control route
High specific stiffness or ESD review PA-CF30 Weight, low CTE, or electrical formulation requirements
Wet dimensional service PA12 or qualified modified grade Lower moisture uptake

Présentation générale de la gamme Nylon

Grade Type Point de fusion Humidité (50% RH) Caractéristique principale
PA6 Aliphatique 220°C 2.7% Résistance, aptitude à la transformation
PA66 Aliphatique 260 °C 2.5% Résistance mécanique, résistance à la chaleur
PA11 D'origine biologique 185 °C 0.8% Souplesse, faible teneur en humidité
PA12 Aliphatique 178 °C 0.7% Absorption d'humidité minimale
PA46 Aliphatique 295 °C 3.5% Résistance maximale à la chaleur
Tableau comparatif des types de nylon
Chaque type de nylon répond à des exigences de performance spécifiques

PA6 : un matériau polyvalent et robuste

Le PA6 est la nuance de nylon la plus couramment utilisée ; elle représente environ 60% de la consommation totale de nylon. Elle offre un excellent équilibre entre résistance, ténacité et aptitude à la mise en œuvre.

Propriétés principales

  • Résistance à la traction : 70-85 MPa
  • Excellente résistance aux chocs
  • Bonne finition de surface et bonne aptitude à la coloration
  • Une fenêtre de transformation plus large que celle du PA66

PA66 : la référence en matière de haute performance

Applications du PA66 dans le secteur automobile
Le PA66 domine les applications automobiles sous le capot

Le PA66 offre une résistance et une rigidité supérieures d'environ 10 à 15% à celles du PA6, ainsi qu'une résistance à la chaleur supérieure. C'est le matériau de choix pour les applications exigeantes.

PA11 et PA12 : les nylons spécialisés

Les PA11 et PA12 se distinguent par leur absorption d'humidité exceptionnellement faible — inférieure à 1%, même à saturation. Cela leur confère une stabilité dimensionnelle remarquable.

Applications du PA11 et du PA12
Les grades PA11 et PA12 se distinguent par leur résistance aux produits chimiques et leur stabilité dimensionnelle

PA46 : le spécialiste des hautes températures

Le PA46 (Stanyl) présente la résistance à la chaleur la plus élevée de tous les nylons aliphatiques, avec un point de fusion de 295 °C.

Base Resin and Reinforcement Are Separate Decisions

PA6-GF20 and PA66-GF20 share the same glass percentage but not the same moisture response, melting range, heat capability, or processing window. The same applies to PA6-CF30, PA66-CF30, and PA12-CF30. Drawings and purchase orders should identify the complete matrix and modification package.

  • Unfilled PA: prioritize toughness, fatigue, wear, surface quality, and easier processing.
  • GF20: use when moderate stiffness and lower shrinkage are needed without moving directly to a higher glass loading.
  • GF30: use for a common structural balance, with gate, weld-line, and warpage review.
  • CF30: use when specific stiffness, low thermal expansion, weight, or an electrical target justifies the premium and processing controls.

Guide de sélection

Exigence Niveau recommandé
Usage général, à prix abordable PA6
Haute température (> 120 °C) PA66, PA46
Environnement humide PA12, PA11
Rigidité maximale PA66-GF30/50

Modified Nylon Grade and Supply Review

Nylon Plastic supplies unfilled and modified PA compounds, with primary article and product support centered on pure PA, PA-GF20, and PA-CF30 routes. Grade review should include the drawing, service conditions, required approvals, annual volume, color, and incumbent specification.

Common Nylon Grade Selection Mistakes

  • Writing only “nylon” or “PA” on the drawing without identifying the matrix and modification.
  • Comparing dry tensile values while the production part will operate in humid or conditioned service.
  • Increasing fiber content before checking whether the real problem is geometry, gate position, weld lines, or creep.
  • Choosing CF30 for maximum stiffness when a GF20 compound already meets the functional requirement at lower cost and processing risk.
  • Assuming a flame, ESD, heat-stabilized, or approved formulation from the family name instead of the exact grade documentation.

Nylon Grade RFQ Checklist

A complete inquiry should identify the preferred PA matrix, reinforcement percentage, annual volume, drawing revision, color, molding process, service temperature, humidity, chemicals, impact, load duration, dimensional state, and regulatory requirements. Include the incumbent grade and failure mode when the request is a replacement project. This information allows the supplier to compare unfilled PA, GF20, GF30, and CF30 without relying on a generic strength ranking.

How Nylon Plastic Reduces Grade-Selection Risk

Buyers often receive quotations that list a resin family but omit the exact modification, conditioning state, or approval package. Nylon Plastic has worked across material modification and finished-product manufacturing since 2005, allowing one project review to connect grade selection with the intended molding, CNC, or 3D-printing route.

  • Product focus: pure PA, PA-GF20, and PA-CF30 can be compared as distinct commercial routes.
  • Custom compounding: formulation review is available when standard grades do not meet stiffness, impact, color, wear, flame, or dimensional requirements.
  • Manufacturing feedback: gate direction, machining deformation, moisture conditioning, or print orientation can be considered before material approval.
  • Buyer documentation: the RFQ can define TDS, COA, compliance, sample, incoming inspection, and lot-approval expectations before volume ordering.

Questions fréquemment posées

Should I choose PA6 or PA66 for injection molding?

PA6 often provides a broader processing window and good toughness, while PA66 is commonly selected for higher strength and thermal margin. Moisture, impact, geometry, approvals, and exact grade data can change the decision.

When should an unfilled nylon grade be replaced with GF20?

Consider GF20 when the unfilled grade cannot meet deflection, creep, shrinkage, or loaded-temperature targets. Validate impact, weld lines, warpage, surface appearance, and tool wear before approval.

What is the difference between GF20 and CF30 nylon?

GF20 uses approximately 20% glass fiber and is generally a more cost-effective moderate reinforcement. CF30 uses approximately 30% carbon fiber and targets higher specific stiffness, lower thermal expansion, or electrical behavior, depending on the formulation.

What must a nylon grade RFQ include?

Include the PA matrix, reinforcement or modification, drawing, volume, service temperature, humidity, chemicals, load, impact, tolerances, color, flame rating, and regulatory requirements.

Lire la suite

Request a Nylon Grade Review

Send the drawing, current material, target properties, annual volume, and operating environment. We can compare the matrix and modification separately before recommending unfilled PA, GF20, GF30, or CF30.

Parlez-nous de votre pièce

Ce champ est requis.
Ce champ est requis.
Ce champ est requis.
Ce champ est requis.
Ce champ est requis.
Ce champ est requis.
Ce champ est requis.
Défiler vers le haut